Products Description
With excellent comprehensive performance, titanium and titanium alloys have become the preferred materials for medical implant products such as artificial joints (hip, knee, shoulder, ankle, elbow, wrist, finger joints, etc.), bone trauma products (intramedullary nails, steel plates, screws, etc.), spinal orthopedic internal fixation systems, dental implants, dental brackets, dental orthopedic wires, artificial heart valves, interventional cardiovascular stents, etc.

The chemical composition shall conform to GR23 grade in ASTM F136, and the H content in pure titanium, Gr5, and Gr5 ELI shall not be greater than 0.010%. During the re-inspection by the Demander, the allowable deviation of chemical composition shall comply with the provisions of ASTM F136.

No cracks, air holes, metal or non-metallic inclusions, or other visible defects are allowed on the transverse macrostructure of medical titanium alloy bars. The transverse microstructure of pure titanium bar in an annealing state shall be uniform, and the grain size shall not be lower than Grade 5. The macrostructure of medical titanium alloy bars in the annealed state shall conform to A1~A9.
The ingots used for the production and processing of materials shall be melted in a vacuum consumable arc furnace or EB furnace plus a vacuum consumable arc furnace, and the melting times shall not be less than two.
As surgical implant materials, titanium and titanium alloys have many advantages, such as low density, high strength, good toughness, good biocompatibility, non-toxic, low elastic modulus, good corrosion resistance, low X-ray absorption, etc., so they play an increasingly important role in medical metal materials.
Products parameters
| OD Size | length Size/mm | Box Size/cm | Stock | Standards |
| 3.0 3.5 4.0 5.0 | 2880~3000 | 302*20*15 | 103PCS | ASTMF136 |
| 6.0 7.0 8.0 8.5 9.0 10.0 | 2500~3000 | 302*20*15 | 180PCS | ASTMF136 |
| 11 12 13 14 15 | 2500~3000 | 302*20*15 | 144PCS | ASTMF136 |
| 16 17 18 19 20 | 2500~3000 | 302*20*15 | 108PCS | ASTMF136 |
| 21 22 25 28 30 | 2500~3000 | 302*20*15 | 108PCS | ASTMF136 |
Product Picture


Our factory

workshop

workshop

workshop
workshop
Titanium and its alloys can be used for the repair and replacement of human hard tissues, or for the repair of cardiovascular and soft tissues, as well as the manufacture of artificial organs. It is a special functional material closely related to human life and health. At present, it has become the preferred metal material for replacement or repair products such as artificial joints, artificial bones, bone fracture fixators, manual bone correction devices, bone marrow nails, artificial heart valves, dental implants, skulls, etc.